Cloudy DAF effluent has several causes, and polymer fixes only some of them. Find the cause, run a flotation jar test, then convert the dose to a pump rate before you order an anionic polymer flocculant.

TL;DR

  • An anionic polymer flocculant bridges conditioned particles into flocs that attach to air bubbles and float off in a DAF.
  • It clears cloudy effluent only when weak flocculation is the cause. Check air, recycle, loading and skimming first.
  • 1-50 ppm is a reference range from one anionic emulsion bulletin; dose basis must be confirmed; not a starting dose for your DAF.
  • Run a jar test that includes flotation. A settling-only test does not predict DAF performance.
  • Too much polymer can make clarity worse, so test doses above and below the apparent best dose.

An anionic polymer flocculant clears cloudy DAF effluent when the solids are not forming flocs that are big and strong enough to catch air bubbles. The polymer chains bridge conditioned particles into larger flocs, which attach to the fine bubbles and rise as float for the skimmer to remove.

It will not fix every hazy weir. If the haze comes from too little dissolved air, an overloaded tank or late skimming, more polymer does not help and can make things worse. Below you will find how to trace the cause at your plant in Muscat or anywhere in Oman, how to test our Flocculant Anionic Polymer DAF (RXSOL-81-8163-220) on your own wastewater, and how to turn a jar-test result into a pump setting.

Why does DAF effluent turn cloudy?

Common causes include unsuitable chemical conditioning, too little dissolved air, too much hydraulic load and solids carryover from the float. Find out which one applies before you touch the polymer dose.

Your first clue is what you see in the tank and at the outlet. Use the table below as a first-check guide.

What you seeLikely areaFirst check
Fine, even haze, very small or no visible flocChemical conditioningCoagulant dose and pH, then whether polymer is reaching the line at the set rate
Floc forms in the flocculator, then breaks into pin flocShear or polymer make-downMixer speed, pump type, valves and pipe bends after the dosing point; lumps or gels in the made-down solution
Good floc that hangs mid-tank and does not riseAir and recycleSaturator pressure, recycle flow and bubble observations
Float breaking up or solids going over the outlet weirHydraulic load or skimmingPlant flow against design, flow split between units, skimmer timing and float removal

Record what you find, change one thing at a time, and check both the clarified water and the float after each change.

How an anionic polymer flocculant improves DAF clarity

The polymer works by bridging: its long chains link many small, already conditioned particles into one larger floc. Larger flocs attach to the fine air bubbles and float to the surface for removal.

Our RXSOL-81-8163-220 is a high molecular weight, medium anionic, water-soluble polymer supplied as a liquid emulsion, and dissolved air flotation is one of its listed uses. Being an emulsion, it must be made down into a dilute solution before it goes into the wastewater.

Visible floc on its own does not guarantee flotation. You still need enough air release, bubble attachment, suitable hydraulic conditions and timely float removal.

When to use an anionic polymer after a coagulant

An anionic polymer can be tested after a coagulant when the coagulant has conditioned the particles but the flocs stay small and weak. The polymer then adds the bridging step that builds them up.

Charge and order of addition depend on your wastewater, so treat them as things to test. Some streams respond better to a different charge or to a changed dosing sequence. Your jar test should compare the existing coagulant alone against coagulant followed by the anionic polymer.

How to run a DAF jar test that predicts flotation

A useful DAF jar test copies your plant's chemical sequence and then floats the sample with air-saturated water. A settling-only jar test does not reliably predict how the DAF will perform.

  1. Take representative samples. Collect wastewater at the DAF inlet at a normal production time. Repeat the test when the wastewater changes, for example after a tank wash or a product change.
  2. Record the sample conditions. Note pH, conductivity, visible oil, suspended solids if you can measure them, and any cleaning discharge that day. Record conditions such as sample temperature, salinity or hardness of make-up water, and oily washdowns; do not assume they are the cause.
  3. Make a fresh polymer stock. One anionic emulsion bulletin recommends a make-down of 0.25-1.0 % before use; the strength and basis for RXSOL-81-8163-220 come from our TDS. Use a low-speed agitator with large blades and check the solution is uniform, with no lumps or gels.
  4. Set up controls. Run one untreated jar and one coagulant-only jar beside the polymer jars.
  5. Run a dose curve. One anionic emulsion bulletin gives 1-50 ppm for wastewater clarification. This is a reference range from one anionic emulsion bulletin; dose basis must be confirmed; not a starting dose for your DAF. Test several doses, including doses above and below the one that looks best, because excess polymer can weaken bridging and flotation.
  6. Copy the plant mixing. Rapid mix, then gentler flocculation, matching your order of addition. One published DAF protocol used 1.5 minutes rapid mix, two gentle stages of 4.5 and 6.5 minutes, and 12.5 minutes flotation. Treat these as an example, not a setting for your plant.
  7. Float, do not settle. Add pressurised air-saturated water. The same example protocol used 600 kPa saturation pressure and 8 % recycle; match your own saturator and recycle where you can.
  8. Measure more than appearance. Draw clarified water from beneath the float and record turbidity. Note float thickness and whether it holds together.

Choose the lowest dose that gives the clarity you need with a firm float, then confirm it at plant scale.

How to convert a jar-test dose into a plant feed rate

Multiply plant flow by the jar dose to get product per hour, then divide by your make-down strength to get the solution pump rate. Keep three numbers apart: active polymer, as-supplied product and liquid volume.

The figures below are illustrative assumptions only. Take the active fraction, density and make-down strength from our current TDS.

  • Plant flow: 50 m³/h
  • Best jar dose: 5 mg/L as active polymer (5 g/m³)
  • Active polymer: 250 g/h (50 m³/h × 5 g/m³)
  • Assumed active fraction of the emulsion: 30 %
  • As-supplied product: 833 g/h (250 ÷ 0.30)
  • Assumed density of the neat emulsion: 1.05 kg/L, giving about 0.79 L/h of neat product
  • Assumed as-supplied make-down of 0.5 % (5 g of product per litre): solution pump rate about 167 L/h (833 ÷ 5)

If your jar dose was worked out on as-supplied product rather than active polymer, skip the active fraction step. Confirm which basis your jar dose used before setting the pump.

What to check when floc forms but effluent stays cloudy

If you can see good floc but the outlet is still cloudy, check air, recycle and hydraulics before changing the chemistry. Leave the polymer dose alone while you check the mechanical side.

Recycle flow supplies the pressurised, air-saturated water. Too little air can leave solids in the effluent. Too much recycle adds internal hydraulic load and turbulence, and flow above design can cause solids carryover.

Compare plant flow against the unit's design flow, especially at peak production. Then check skimmer timing and float removal.

Trial request checklist for Oman plants

Send us the details below and we can match the product and trial plan to your DAF.

  • Average and peak flow to the DAF
  • Wastewater source and composition, with influent suspended solids and oil and grease if measured
  • pH, temperature and conductivity at the inlet
  • Existing coagulant and polymer, with current doses
  • Recycle flow and saturator pressure
  • Current effluent turbidity and the target you need to meet
  • What you see: bubbles, floc size, float condition
  • Representative samples, if you can send them
ItemDetail
Part numberRXSOL-81-8163-220
FormHigh molecular weight, medium anionic, water-soluble polymer in emulsion form
ApplicationFlocculant for dissolved air flotation (listed application)
Reference dose (product class)1-50 ppm for wastewater clarification: reference range from one anionic emulsion bulletin; dose basis must be confirmed; not a starting dose for your DAF. Refer to our TDS and jar test
Reference make-down (product class)0.25-1.0 % from one anionic emulsion bulletin; strength and basis for this product from our TDS
StorageKeep containers closed; protect from frost and moisture
TDS and SDSOn request; follow the SDS for handling, PPE, spills and transport

Where to buy anionic polymer flocculant in Muscat and Oman

Muscat Chemical (Muscat & Barka for Business Trading), Barka Industrial Area, Sultanate of Oman, supplies RXSOL-81-8163-220 with its current TDS and SDS. Call +968 77333599 or message us on WhatsApp.

We deliver from our Barka warehouse to plants across Muscat. For DAF units in the Sohar industrial area, the same product is listed on Sohar Chemical for northern deliveries. Buyers elsewhere in Oman can also find it on Oman Chem. Browse our other treatment chemicals on the products page.

To start a trial, send your plant details through our quote request page or on WhatsApp at +968 77333599, and we will reply with the TDS, SDS and a quotation.

Need Flocculant Anionic Polymer DAF? Ask us for a quote, the TDS or the MSDS. Delivery across Oman from our Barka warehouse.

Request a quote · WhatsApp us

Frequently asked questions

Why is my DAF effluent cloudy?

Common causes include unsuitable chemical conditioning, too little dissolved air, hydraulic load above design, and solids carrying over from the float. Check what you see in the tank first: fine haze points to chemistry, floc hanging mid-tank points to air and recycle, and solids over the weir point to loading or skimming.

Can too much polymer cause cloudy DAF effluent?

Yes. Excess polymer can weaken bridging and flotation, so clarity can get worse past the best dose. Your jar test should include doses above and below the dose that looks best.

How do I choose the right polymer dose for DAF wastewater?

Run a flotation jar test on representative samples with untreated and coagulant-only controls and a dose curve. One anionic emulsion bulletin gives 1-50 ppm for wastewater clarification; this is a reference range only, its dose basis must be confirmed, and it is not a starting dose for your DAF. Pick the lowest dose that gives the clarity you need with a firm float, then confirm it at plant scale.

How do poor make-down and too much mixing affect floc?

Incomplete make-down leaves lumps or gels that do not mix evenly into the wastewater. Too much shear can damage the polymer or break the floc. Make down slowly with a low-speed, large-blade agitator and check the solution looks uniform.

What should an Oman plant send when requesting a polymer trial?